Alloy 276 Stainless Steel Coil Tubing Mutengo
Hastelloy C276 Chemical Kuumbwa
SIHE STAINLESS STEEL ndeyechizvino-zvino mutekinoroji yekurongedza Zvinhu zvinoenderana neInternational Standard uye zvitsva zvitsva.Isu tinoisa kukoshesa kwakawanda paKurongedza uye kunyora mazita kuti Tipe Zvigadzirwa Zvemhando yepamusoro kune Mutengi Wedu Wepamba uye Wepasi Pose.Hastelloy C276 Fittings yakanyatso kurongedzerwa nezvikamu zvePlastiki foils uye Bubble yakaputirwa uye yakanyatsoiswa mumabhokisi emapuranga.
Ndokumbira tifonere kuti titarise zvakadzama mamwe mashandisirwo ayo anosanganisira kumwe kuenzanisa corrosion resistance data, midhiya, kudzikisira uye tembiricha.Kuti uwane rumwe ruzivo nezve SIHE Stainless STEEL 's Pipe uye Piping Systems, ndapota ona yedu Hastelloy C276 pombi uye Hastelloy C276 Tube mapeji.
Hastelloy C276 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Balance | 0.010 max | 15.00 - 17.00 | 1.00 max | 0.08 max | 4.00 - 7.00 | 0.04 max | 0.03 max | 2.5 max | 14.50 - 16.50 |
Hastelloy C276 Mechanical Properties
Yakajairika Kamuri Tembiricha Tensile Zvivakwa zveAnealed Material
Product Form | Tensile (ksi) | .2% Goho (ksi) | Elongation % |
Alloy C276 Bar | 110.0 | 52.6 | 62 |
Alloy C276 Plate | 107.4 | 50.3 | 67 |
Alloy C276 Sheet | 115.5 | 54.6 | 60 |
Alloy C276 Tube &Alloy C276 Pipe | 105.4 | 45.4 | 70 |
Hastelloy C276 Melting Point
Zvinhu Zvenyama | °F | British Units | °C | Metric Units |
Density | 72 | 0.321 lb./in.(3) | 22 | 8.89 g/cm(3) |
Melting Range | 2415- | 1323- | ||
Zvemagetsi | 75 | 51 microhm-mukati. | 24 | 1.30 microhm-m |
Mean Coefficient | 75-200 | 6.2 microin./in.-°F | 24-93 | 11.2 X 10(-6)m/mK |
75-400 | 6.7 microin./in.-°F | 24-204 | 12.0 X 10(-6)m/mK | |
75-600 | 7.1 microin./in.-°F | 24-316 | 12.8 X 10(-6)m/mK | |
75-800 | 7.3 microin./in.-°F | 24-427 | 13.2 X 10(-6)m/mK | |
75-1000 | 7.4 microin./in.-°F | 24-538 | 13.4 X 10(-6)m/mK | |
75-1200 | 7.8 microin./in.-°F | 24-649 | 14.1 X 10(-6)m/mK | |
75-1400 | 8.3 microin./in.-°F | 24-760 | 14.9 X 10(-6)m/mK | |
75-1600 | 8.8 microin./in.-°F | 24-871 | 15.9 X 10(-6)m/mK | |
75-1700 | 8.9 microin./in.-°F | 24-927 | 16.0 X 10(-6)m/mK | |
Thermal | -270 | 50 Btu-in/ft²-hr-°F | -168 | 7.2 W/mK |
-100 | 60 Btu-in/ft²-hr-°F | -73 | 8.6 W/mK | |
0 | 65 Btu-in/ft²-hr-°F | 32 | 9.4 W/mK | |
100 | 71 Btu-in/ft²-hr-°F | 38 | 10.2 W/mK | |
200 | 77 Btu-in/ft²-hr-°F | 93 | 11.1 W/mK | |
400 | 90 Btu-in/ft²-hr-°F | 204 | 13.0 W/mK | |
600 | 104 Btu-in/ft²-hr-°F | 316 | 15.0 W/mK | |
800 | 117 Btu-in/ft²-hr-°F | 427 | 16.9 W/mK | |
1000 | 132 Btu-in/ft²-hr-°F | 538 | 19.0 W/mK | |
1200 | 145 Btu-in/ft²-hr-°F | 649 | 20.9 W/mK | |
1400 | 159 Btu-in/ft²-hr-°F | 760 | 22.9 W/mK | |
1600 | 173 Btu-in/ft²-hr-°F | 871 | 24.9 W/mK | |
1800 | 185 Btu-in/ft²-hr-°F | 982 | 26.7 W/mK | |
2000 | 195 Btu-in/ft²-hr-°F | 1093 | 28.1 W/mK |
Hastelloy C276 Yakaenzana
STANDARD | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST |
Hastelloy C276 | N10276 | 2.4819 | - | NiMo16Cr15W | NW 0276 | - | ХН65МВУ |
Zvigadzirwa Zvinotsanangurwa
ASTM B622, B829 / ASME SB622, SB829 / NACE MR0175
Size Range
Kunze Diameter (OD) | Kukora Kwemadziro |
.250”–.500” | .035”–.065” |
Kutonhora kwapera uye kupenya annealed chubhu.
Kemikari Zvinodiwa
Alloy C276 (UNS N10276)
Kuumbwa %
Ni Nickel | Cr Chromium | Mo Molybdenum | Fe Iron | W Tungsten | C Carbon | Si Silicon | Co Cobalt | Mn Manganese | V Vanadium | P Phosphorous | S Sulfur |
57.0 min | 14.5–16.5 | 15.0–17.0 | 4.0–7.0 | 3.0–4.5 | 0.010 max | 0.08 max | 2.5 max | 1.0 max | 0.35 max | 0.04 max | 0.03 max |
Dimensional Tolerances
OD | OD Kushivirira | Kushivirira Kwemadziro |
.250"–.500" | +.004”/-.005” | ± 15% |
Mechanical Properties
Goho Simba: | 41 ksi min |
Tensile Simba: | 100 ksi min |
Elongation (min 2"): | 40% |